Mechanical Properties Metric English Comments
Flexural Strength 406 MPa
58900 psi
ASTM D790
Quantum Composites QC-8850 43% Glass Fiber Reinforced Polyester Hybrid SMC
QC-8850 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and ..
Flexural Strength 406 MPa
58900 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66
LNP* THERMOCOMP* RC006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 406 MPa
58900 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66 (Asia Pacific)
LNP* Thermocomp* RC006 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.