Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 40.14 MPa | 5822 psi | ASTM D790 |
Asia Technology Pioneers CAP 101 PP Nanocomposite Description: CAP101 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |