Mechanical Properties Metric English Comments
Flexural Strength 4.00 MPa
580 psi
ISO 178
Styrolution Styroflex® 2G 66 SBC
Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o..
Flexural Strength 4.00 MPa
580 psi
ASTM D790
A. Schulman POLYFORT™ PX 1040
Information provided by A. Schulman.
Flexural Strength 4.00 MPa
580 psi
ASTM D790
A. Schulman POLYFORT™ PX 1040
Information provided by A. Schulman.
Flexural Strength 4.00 MPa
580 psi
ASTM D790
A. Schulman POLYFORT™ PX 1040
Information provided by A. Schulman.
Flexural Strength 4.00 MPa
580 psi
ASTM D790
A. Schulman POLYFORT™ PX 1040
Information provided by A. Schulman.
Flexural Strength 4.00 MPa
580 psi
ASTM D790
A. Schulman POLYFORT™ PX 1040
Information provided by A. Schulman.
Flexural Strength 4.00 MPa
580 psi
SAE J949
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (7 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 4.00 MPa
580 psi
SAE J949
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness)
AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 4.00 MPa
580 psi
SAE J949
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness)
AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 4.00 MPa
580 psi
SAE J949
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (6 mm Molded Thickness)
AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 4.00 MPa
580 psi
SAE J949
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (6 mm Molded Thickness)
AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 4.00 MPa
580 psi
ASTM D790
A. Schulman POLYFORT™ PX 1040