Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 57.7 MPa | 8370 psi | ASTM D790 |
PolyOne Maxxam™ PPH-40T Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 57.7 MPa | 8370 psi | ASTM D790M |
DSM Somos® WaterClear® 10110 Epoxy Resin for Stereolithography
(discontinued **) DescriptionDSM Somos® 10110 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us.. |