Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 560 MPa @Temperature 538 °C |
81200 psi @Temperature 1000 °F |
|
McDanel Advanced Ceramics SiAlON Information provided by McDanel Advanced Ceramic Technologies. |
|||
Flexural Strength | >= 560 MPa | >= 81200 psi | Limit of elasticity in Bending |