Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 3.79 MPa | 550 psi | ASTM D790 |
AdvanSource Biomaterials ChronoFlex® C 55D Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |