Polymer Property : Flexural Strength = 5310 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 36.6 MPa
5310 psi
ASTM D790-95
Multibase Multi-Flex® TPO D-6500
Multi-Flex® D 6500 is well suited for TPO extrusion applications and certain high value molded parts for the telecommunications industry.Data provided by Multibase.