Flexural Strength 530 MPa
76900 psi
Lehmann & Voss LUVOCOM® 20/XCF/35 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Flexural Strength 530 MPa
76900 psi
Ceradyne Ceralloy® 7712 Al2O3-SiC
Applications:slot mode absorbersInformation provided by Ceradyne Company