Mechanical Properties Metric English Comments
Flexural Strength 36.5 MPa
5290 psi
1.0 in/min; 0.125" thickness; ASTM D-790
Chevron Phillips K-Resin® KR03BR SBC  (discontinued **)
K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:BottlesMolded boxes and containersMedical devicesPortion packagesBlister packagingFeatures:Good stiffnessGood formabilityGood toughnessExcelle..