Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 5102 MPa | 740000 psi | Hardening Temperature- 1175°C, Tempering Temperature- 565°C |
Crucible Steel CPM® Rex® T15(HS), AISI T15 High Speed Steel Rex® T15(HS) CPM Rex T15 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed containing high vanadium for excellent abrasion resistance, and cobal.. |