Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 5.30 - 5.40 MPa | 769 - 783 psi | |
FiberNide Nickel Aluminide Foam Atomic 20% Aluminum Description: This Nickel aluminide foam has excellent high temperature strength, oxidation resistance, and conductivity. This unique combination of properties makes this foam particularly suitable f.. |
|||
Flexural Strength | 5.30 MPa @Thickness 19.0 mm |
769 psi @Thickness 0.750 in |
ASTM D790 |
3A Composites Core Materials AIREX® PXc.245 Fiber-Reinforced Structural Foam AIREX® PXc is a closed-cell, fiber reinforced polymer foam with very high mechanical properties ideally suited as core material for structurally loaded sandwich applications. The sophisticated manu.. |