Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 493 MPa @Thickness 3.17 mm |
71500 psi @Thickness 0.125 in |
LW |
Industrial Laminates/Norplex MC511A Glass Fabric Description: MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer's exacting standards where higher strength at elevated temperatures ar.. |