Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 49.01 MPa | 7109 psi | ASTM D790 |
Network Polymers NPS 90-0304 Super High Impact Polystyrene Description: Injection Molding GradeInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 49.01 MPa | 7109 psi | ASTM D790 |
Network Polymers NPS 90-0304 F Super High Impact Polystyrene Description: Injection Molding GradeInformation provided by Network Polymers Inc. |