Polymer Property : Flexural Strength = 4800 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 4800 MPa
696000 psi
HRC 66
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel
Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug..