Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.333 MPa | 48.3 psi | 16 hour silo aging time, 20 kg/m^3 |
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |