Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 47.1 MPa | 6830 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0190H ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 47.1 MPa | 6830 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0190H ABS, Unreinforced Information provided by Samsung Cheil Industries. |