Mechanical Properties Metric English Comments
Flexural Strength 318.9 MPa
46250 psi
ASTM D790
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced
Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..