Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 308.98 MPa | 44814 psi | Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D790 |
Fibre Glast EZ Poxy EZ10 / EZ83 Epoxy
(discontinued **) Information provided by Fibre Glast Developments Corporation. |