Polymer Property : Flexural Strength = 44700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 308 MPa
44700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EC004XXQ PEI
LNP* THERMOCOMP* EC004XXQ is a compound based on Polyetherimide containing 20% Carbon Fiber.
Flexural Strength 308 MPa
44700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp LC008 PEEK (Europe-Africa-Middle East)
LNP* Thermocomp* LC008 is a compound based on Polyetheretherketone resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.