Polymer Property : Flexural Strength = 4320 psi
Polymer Property :
Flexural Strength =
4320 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Strength
29.8
MPa
4320
psi
chs 0.05 in/min; ASTM D790
Diamond Polymers DIAMALOY WPE 2000 Wood Filled HDPE
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.