Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 291 MPa | 42200 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA 6/12 LNP THERMOCOMP* IF006 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber. |
|||
Flexural Strength | 291 MPa | 42200 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 653 Nylon 6/6, Carbon Fiber Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 291 MPa | 42200 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RX00327 PA 66 LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural. |