Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 29.1 MPa | 4220 psi | ASTM D790 |
Quadrant EPP Borotron® HD050 5% Boron-filled Polyethylene (ASTM Product Data Sheet) |
|||
Flexural Strength | 29.1 MPa | 4220 psi | ASTM D790 |
PolyOne Geon™ Vinyl Cellular E2000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 29.1 MPa | 4220 psi | ASTM D790 |
PolyOne Geon™ Vinyl Cellular E2001 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 29.1 MPa | 4220 psi | ASTM D790 |
PolyOne Geon™ Vinyl Cellular E2010 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Physical Properties were measured on flat cellular profiles with a 0.59 specific gravity natural compound.Information provided by PolyOne |