Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 41.62 MPa | 6036 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 41.62 MPa | 6036 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 41.62 MPa | 6036 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 41.62 MPa | 6036 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 41.62 MPa | 6036 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Strength | 41.62 MPa | 6036 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |