Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 404 MPa | 58600 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00CEXS PA 66 LNP* VERTON* RV00CEXS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |