Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 276 MPa | 40100 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF33 L UV 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and UV Stabilizer Features: Lubricated and Good UV ResistanceInforma.. |
|||
Flexural Strength | 276 MPa | 40100 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF35 LE 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant Features: Lubricated and Low ExtractablesInformation provided by TP .. |
|||
Flexural Strength | 276 MPa | 40100 psi | ASTM D790 |
Techmer ES HiFill® PA6 B3 EG6 MB Colors Availability: North AmericaForms: PelletsAppearance: Colors AvailableTPCI# 6101102Information provided by TP Composites, Inc. |