Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 4.83 MPa @Temperature 316 °C |
700 psi @Temperature 600 °F |
|
Greene Tweed Arlon® 1000 Polyketone Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |