Flexural Strength 274.68 MPa
39839 psi
ASTM D790
E-Polymers SEPAZ® V235A 35% Glass Fiber Reinforced PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..
Flexural Strength 274.68 MPa
39839 psi
ASTM D790
E-Polymers SEPAZ® LA30 PA66 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..