Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2300 - 2700 MPa | 334000 - 392000 psi | |
China Tungsten Z25 Tungsten Carbide for Mining Purposes Of high toughness and wear resistance as well as good versatility, for rotary hammer rock drill bits and pillar bit drills, for f14~f16 medium hard and hard rock formations.Information provided by C.. |