Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 265.1 MPa | 38450 psi | ASTM D790 |
Polymer Resources NY6-G20 Nylon 6, 20% Glass Reinforced Nylon 6, 20% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |