Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 382 MPa | 55400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RC006XXH PA 66 LNP* THERMOCOMP* RC006XXH is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
Flexural Strength | 382 MPa | 55400 psi | |
Astro Met AmAlOx 68 Alumina - Aluminum Oxide General Description:AmAlOx 68 alumina (Astro Met Aluminum Oxide) is a high purity 99.8% aluminum oxide (alumina) ceramic which has been developed and optimized for maximum wear resistance and corros.. |