Mechanical Properties Metric English Comments
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
PolyOne Maxxam™ MD 4245-59770 Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
PolyOne Maxxam™ PPC-20T Black Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
PolyOne Maxxam™ PPC-30T UV EXT 1148 Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Multibase Nylex™ 2185 FR Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric..
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
ITW Devcon Plastic Steel® Metal Repair (A), Dark Grey
Information provided by ITW Devcon
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Techmer ES HiFill FR® ASA FR-2 WT
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc.
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Techmer ES HiFill FR® ASA FR-2A WT209
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant, Good Toughness and Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc.
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Techmer ES HiFill® HIPS 484 GY
Availability: North AmericaForms: PelletsAppearance: GreyInformation provided by TP Composites, Inc.
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Techmer ES HiFill® HIPS LE BK
Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 8813148Information provided by TP Composites, Inc.
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Techmer ES HiFill® HIPS WT
Availability: North AmericaForms: PelletsAppearance: WhiteInformation provided by TP Composites, Inc.
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Techmer ES HiFill® HIPS BK
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Total PSI 945 Polystyrene
Polystyrene 945 is designed for injection molding applications requiring superior toughness. This polymer is a high impact polystyrene with excellent gloss and falling dart properties. The impact an..
Flexural Strength 38.6 MPa
5600 psi
chs 0.05 in/min; ASTM D790
Diamond Polymers Centrex® 485 Sheet Extrusion Grade
Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it..
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Entec Hyrene® PS-HI 3/2 High Impact Polystyrene
Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Asahi Kasei Thermofil P6-9900-0570 Unfilled, Flame Retardant, Heat Stabilized
Information provided by Asahi Thermofil
Copyright © lookpolymers.com All Rights Reserved