Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 378 MPa | 54800 psi | ASTM Test |
BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Dry) Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldabil.. |