Flexural Strength 37.3 MPa

@Thickness 3.20 mm
5410 psi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 562 Flame Retardant Polystyrene
Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Low specific gravity Processing Injection moldingApplications Large size T.V. Cabinets Aud..
Flexural Strength 37.3 MPa

@Thickness 3.20 mm
5410 psi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 564 Flame Retardant Polystyrene
Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Processing MoldingApplications Large size T.V. Cabinets VCR cabinets Electrical boxes, ele..