Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 364 MPa | 52800 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow. |
|||
Flexural Strength | 364 MPa | 52800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EC008PXQ PEI LNP* THERMOCOMP* EC008PXQ is a compound based on Polyetherimide containing 40% Carbon FIber. Added features include: Electrically Conductive, Exceptional Processing |
|||
Flexural Strength | 364 MPa | 52800 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RC006XXH PA 66 LNP* THERMOCOMP* RC006XXH is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |