Mechanical Properties Metric English Comments
Flexural Strength 250.0 MPa

@Thickness 3.17 mm
36260 psi

@Thickness 0.125 in
ASTM D790
Polyram PB330I8 Nylon 6, 40% Mineral/Glass Filled Heat Stabilized
Information provided by Polymer Technology and Services, LLC (PTS).