Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 36.9 MPa | 5350 psi | ASTM D790-95 |
Multibase Multi-Pro® 1012 C BLK Medium Impact Mineral Filled Polypropylene Mineral filled PP compound for interior automotive applications. Product meets GMP PP 056 and EBG-M4 D605-A specifications. Ash is 10%.Data provided by Multibase. |