Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 36.2 MPa | 5250 psi | ASTM D790 |
Quadrant EPP PROTEUS® EURO-GRAY Copolymer Polypropylene |
|||
Flexural Strength | 36.2 MPa | 5250 psi | ASTM D790 |
Chase Plastics CP Pryme® N300HSL (COND, 50% RH) Nylon 6 (Utility Grade), Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 36.2 MPa | 5250 psi | ASTM D790 |
Chase Plastics CP Pryme® N300L (COND, 50% RH) Nylon 6 (Utility Grade), Internally Lubricant Information provided by Chase Plastics. |