Mechanical Properties Metric English Comments
Flexural Strength 2250 MPa
326000 psi
China Tungsten YG16C Cemented Tungsten Carbide for Mining Purposes
For oil cone drill bits for medium soft and medium hard rocks.Information provided by China Tungsten