Mechanical Properties Metric English Comments
Flexural Strength 298.72 MPa
43325 psi
ASTM D790
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
Flexural Strength 298.72 MPa
43325 psi
ASTM D790
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
Flexural Strength 298.72 MPa
43325 psi
ASTM D790
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
Flexural Strength 298.72 MPa
43325 psi
ASTM D790
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
Flexural Strength 298.72 MPa
43325 psi
ASTM D790
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
Flexural Strength 298.72 MPa
43325 psi
ASTM D790
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.