Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 298 MPa | 43200 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 (Asia Pacific) LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing Flame Retardant, Long Glass Fiber, Long Glass. Added features of this material include: Easy Molding. |