Polymer Property : Flexural Strength = 29740 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 205.0 MPa
29740 psi
Shinil Chemical SHINCON PES-CNT LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..