Mechanical Properties Metric English Comments
Flexural Strength 29.6 MPa
4300 psi
ASTM D790
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE
Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri..
Flexural Strength 29.6 MPa
4300 psi
ASTM D790
Americas Styrenics EB6400 High Impact Polystyrene
Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it..