Flexural Strength 28.6 MPa
4150 psi
ASTM D790
Entec Hyrene® PS-HI 3/3 High Impact Polystyrene
Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec