Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1880 MPa | 273000 psi | |
China Tungsten YW2 Tungsten Carbide for Cutting Tools Wear resistance second to YW1 yet strength comparatively higher and resistant to high impact load. Roughing and medium machining of ordinary steel cst irons as well as refractory steel, manganese st.. |