Polymer Property : Flexural Strength = 2700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 18.6 MPa
2700 psi
ASTM D790
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet)
Flexural Strength 18.6 MPa
2700 psi
Parallel
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..
Flexural Strength 18.6 MPa
2700 psi
ASTM D790
Ensinger Tecatron® XP-73 Compression Molded PPS Compound, 60% PTFE Seal Material
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..