Polymer Property : Flexural Strength = 26607 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 183.45 MPa
26607 psi
ASTM D790
E-Polymers SEPAZ® C230GI 30% Glass Fiber Reinforced Good Impact LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..