Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2520 MPa | 365000 psi | |
China Tungsten YG8 Tungsten Carbide for Cutting Tools High strength in use ,impact and shock resistance higher than YG6,but wear resistance and cutting speed comparatively lower. Roughing of cast irons non ferrous metals and their alloys as well as non.. |