Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 25.46 MPa | 3692 psi | ASTM D790 |
Asia Technology Pioneers CAP 501 PP Nanocomposite Description: CAP501 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |
|||
Flexural Strength | 25.46 MPa | 3692 psi | ASTM D790 |
Asia Technology Pioneers CAP 502 PP Nanocomposite Description: CAP502 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |