Polymer Property : Flexural Strength = 24750 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 170.6 MPa
24750 psi
ASTM D790
PolyOne Edgetek® PS-20GF/000 Polybutylene Terephthalate (PBT), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.