Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 170.0 MPa | 24650 psi | ASTM D790 |
Styron EMERGEâ„¢ 8702 Polycarbonate EMERGEâ„¢ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced, polycarbonate resin. This resin contains no bromide, chloride, or phosphate additives. It is a medium flow PC re.. |
|||
Flexural Strength | 170.0 MPa | 24650 psi | ASTM D790 |
Aclo Accutech Polycarbonate POL051G20L Glass Reinforced |